WELDING PROCEDURE SPECIFICATION (WPS) (D1.2 ALUMINUM) QUALIFIED BY TESTING

by user

on
Category: Documents
19

views

Report

Comments

Transcript

WELDING PROCEDURE SPECIFICATION (WPS) (D1.2 ALUMINUM) QUALIFIED BY TESTING
STATE OF FLORIDA DEPARTMENT OF TRANSPORTATION
675-070-06
MATERIALS
05/15
WELDING PROCEDURE SPECIFICATION (WPS)
(D1.2 ALUMINUM) QUALIFIED BY TESTING
Contractor/Organization:
BACKING
Type:
Removed:
WELDING PROCESS(ES)
Process:
Process:
Electrode: (GTAW):
WELDING PROCEDURE
Specification No:
Date:
By:
Revision:
Date:
By:
Authorized By:
Date:
Supporting PQR No(s):
POSITION
Position of Groove:
Fillet:
Welding Progression (Forehand/Backhand):
Vertical Welding (Upward/Downward):
TECHNIQUE
Stringer or Weave Bead:
Orifice or Gas Cup Size:
Oscillation:
Contact Tube to Work Distance:
Single Pass or Multipass (per side):
Tungsten Extension:
Method of Backgouging:
Other:
POSTWELD HEAT TREATMENT
Original Temper:
Final Temper:
Temp:
Time:
Quench:
PREHEAT
Preheat Temperature:
Interpass Temperature:
FOR FDOT CONSULTANT USE ONLY
Permanent:
Other:
*Type:
*Type:
*Manual, Automatic, Polarity Pulsed, etc.
BASE METALS
M No.:
Alloy & Temper:
FILLER METAL
F-No.:
Size of Electrode:
Type of Electrode:
Mfg. Trade Name:
SHIELDING GAS
Shielding Gas(es):
Percent Composition:
Flow Rate:
Other:
CLEANING
Initial Cleaning Oxide:
Initial Cleaning Oil & Dirt:
Interpass Cleaning:
Thickness:
to
AWS No. (Class):
WELDING PROCESS
Pass No.
Welding
Process
Amps
Volts
Travel Speed
FOR CERTIFIED WELDING INSPECTOR (CWI) USE ONLY
Signature
Date
JOINT GROOVE DESIGN SKETCH
WELDING SEQUENCE SKETCH